By C.C. Sullivan and Barbara Horwitz-Bennett | May 3, 2013

As experienced designers, contractors, and owners know, most paint and coating problems are correctable, but some are especially stubborn to address. The following is a partial compendium of typical failure modes and methods for addressing the problem, as provided by paint and coatings manufacturer Benjamin Moore & Co. (www.benjaminmoore.com):

 

1. Surface imperfections.

There are many types of imperfections that can be visible on painted or sealed surfaces. Alligatoring occurs when the paint film takes on the appearance of alligator hide. (A similar problem is known as wrinkling, which appears as a rough creased or crinkled pattern.) Alligatoring usually occurs when a topcoat is applied before an undercoat is dry, or if an alky enamel or other hard, rigid coating is applied over a latex primer or another more flexible finish layer. Some oil-based coats will lose elasticity as they age, causing this familiar cracking pattern.

 

2. Blistering.

Blistering (or bubbling) is caused by a localized loss of adhesion and lifting of the paint film from the underlying surface, sometimes when solvent gas expands on sunny façades. Blistering tends to occur in fresh coats of paint.

Both problems require removing as much paint as possible and repainting. However, blistering can immediately reappear if the problem is caused by moisture; to mitigate this problem, the contractor should repair loose caulk and retrofit drainage and drying details, if possible. Installing vents or exhaust fans can also reduce moisture by evaporation before it wets enclosure materials.

For alligatoring, most paint contractors will recommend completely remove the existing oil paint by using a heat gun, scraping, and sanding. After priming the reworked surface with a high-quality latex or oil-based primer, the area can then be recoated with exterior latex or similar paint.

 

3. Flaking and chalking.

In some cases, a painted or coated surface will exhibit a loose powder or flaking surface. These problems are caused by decomposing paint and are different from efflorescence or mottling, which display white, crusty mineral salt deposits that have leached from mortar, concrete, or masonry surfaces behind the paint. A similar problem known as frosting is often seen on dark paints and coatings; in this case, a white discolored substance appears on the surface, similar to salt staining.

Chalking paint may be washed by rain and cause patterns, or it may wash across other surfaces, an effect called chalk rundown.

 

4. Miscoloring and staining.

Other sources of miscoloration on exterior and interior surfaces include nailheads and other penetrations that leach a rust-colored stain onto a surface, which often trails down from the location of the hardware. Mildew appears as black, gray, or brown spots or areas on the paint film or caulk bead.

 

5. Surfactant leaching.

Another source of undesired color change is surfactant leaching, in which concentrated, water-soluble ingredients in latexes seep to the paint surface, often creating a brownish blotchy or shiny appearance. Tannin staining can also be a brownish or tan discoloration on the paint surface, caused by wood tannins that leach through the paint film.

When applied properly onto suitably prepared substrates, architectural coatings will rarely exhibit these kinds of failures. Even better, when integrated into a thoughtful sustainability program, paints and coatings can be a partner in effective building designs that promote improvements to project economics and social considerations as well as protecting the environment.

Related Stories

| Jun 8, 2012

Allsteel names Kris Yates to head architectural products group

Yates is responsible for the start up, launch and ongoing sales and marketing of Allsteel’s new Beyond movable walls.

| Jun 8, 2012

Chestnut Hill College dedicates Jack and Rosemary Murphy Gulati complex

Casaccio Yu Architects designed the 11,300-sf fitness and social complex.

| Jun 6, 2012

KPF designs tower for Yongsan IBD

The master plan, created by Studio Daniel Libeskind, is a dynamic urban environment containing contributions from 19 different architects practicing in diverse locations around the globe.

| Jun 6, 2012

SOM urges Chicago tenants to partner with landlords to cut energy use

Tenants can exceed building energy challenge targets recently announced by Mayor Emanuel.

| Jun 6, 2012

KLMK Group awarded contract with Parkland Health & Hospital System in Texas

KLMK will also provide planning guidance in all aspects of the project related to facility activation.

| Jun 5, 2012

Hoffman Architects Arbuckle elected president of New York/Tri-State DOCOMOMO

As chapter president, Arbuckle will guide and oversee the organization's efforts on behalf of Modern buildings and sites, and he will act as the main spokesperson for the organization. 

| Jun 4, 2012

Brownfield goes green

Chicago Center for Green Technology uses high-speed, energy-efficient hand dryers to share its green message and earn LEED credits.

| Jun 4, 2012

KBE Building and CTA Construction awarded Project of the Year from CMAA

Award given for work done on the renovation of Beverly High School in Beverly, Mass.

| Jun 4, 2012

Pressley promoted to Senior VP and CIO at Hill International

Pressley will be responsible for managing all of Hill's information technology systems and software worldwide.

boombox1
boombox2
native1

More In Category




halfpage1

Most Popular Content

  1. 2021 Giants 400 Report
  2. Top 150 Architecture Firms for 2019
  3. 13 projects that represent the future of affordable housing
  4. Sagrada Familia completion date pushed back due to coronavirus
  5. Top 160 Architecture Firms 2021